Polyester dipped cord fabric
Fabric style | 18 PDU-P | 21 PDU-P | 27 PDU-P |
Cord yarn structure, dtex | 1480х1х2 | 1670х1х2 | 2200х1х2 |
Tensile strength, N , min | 178,0 | 200,0 | 265,0 |
Thickness, mm | 0,63±0,03 | 0,63±0,03 | 0,80±0,03 |
Stiffness, cN | 90-190 | ||
Twist direction | ZZS | ||
Hot air shrinkage (tº = 160° С, t = 20 min) % | 2,0±0,5 | ||
Elongation % - at load - at load - at break |
(20Н) 1,8±0,5 (39Н) 3,5±0,6 17,0±2,0 |
(39Н) 2,8±0,5 (90Н) 5,9±1,0 17,0±2,0 |
(45Н) 2,2±0,5 (90Н) 5,7±1,0 17,0±2,0 |
Adhesion, N, min | 137 | 150 | 157 |
Twist per 1 m - single twist - cord twist |
380±20 370±20 |
350±15 350±15 |
325±15 325±15 |
Total number of ends per 10 cm, pcs - by warp - by weft |
115±1 8±1 |
80±1 8±1 |
92±1 8±1 |
Dip pick up ,% | 3,0±1,0 | 2,4±1,0 | 3,0±1,0 |
Fabric width, cm | 140±2,0 | ||
Number of ends per fabric width, pcs | 1613 | 1120 | 1288 |
Nominal linear density of cotton-PA 6.6 weft yarn, tex | 22 | ||
Actual moisture, %, max | 0,8 |
PACKING
Dipped cord fabric preliminarily wound on a shell is packed in the way as follows:
- a roll is wrapped up with foamed polyethylene of 3 mm thickness. On each roll end there are put two cardboard circles with bags consisting moisture absorbing substance preliminarily fixed on it. A roll together with a shell is wrapped up with black polyethylene stretch-foil of 23 mm thickness and 15-25 revolutions of packing machine and a case of polypropylene industrial fabric is put on it.
TRANSPORTATION
Cord fabric is carried in 40’ containers, boxcars and trucks